PDMAEMA based gene delivery materials
Volume 15, Issue 9, Page 388–393
| Seema Agarwal, Yi Zhang, Samarendra Maji, Andreas Greiner
Gene transfection is the transfer of genetic material like DNA into cells. Cationic polymers which form nanocomplexes with DNA, so-called non-viral gene vectors, are a highly promising platform for efficient gene transfection. Despite intensive research efforts and some of the on-going clinical trials on gene transfection, none of the existing cationic polymer systems are generally acceptable for human gene therapy. Since the process of gene transfection is complex and puts different challenges and demands on the delivery system, there is a strong requirement for the design and development of a multifunctional system in a simple way. This review will discuss recent efforts in design, synthesis, and performance of poly(2-dimethylaminoethyl methacrylate) (PDMAEMA) nanocomplexes with DNA.