"What is exciting about our new work is that we've shown that we can dial the degree of hysteresis to identify designs in which these proteins will stick together readily, and once those associations emerge, it becomes very difficult to break them."Felipe Garcia Quiroz, Rockefeller University

Biomedical engineers from Duke University have demonstrated that they can create stable materials from engineered disordered proteins by altering the environmental triggers that cause them to undergo phase transitions.

This discovery shines a light on previously unexplored behaviors of disordered proteins and allows researchers to create novel materials for applications in drug delivery, tissue engineering, regenerative medicine and biotechnology. The engineers report their discovery in a paper in Science Advances.

Proteins function by folding into three-dimensional shapes that interact with different biomolecular structures. Researchers previously believed that proteins needed to fold into a specific fixed shape in order to function. But in the past two decades, engineers seeking to create novel materials for biomedical applications have turned their attention to intrinsically disordered proteins (IDPs), which dynamically shift among a wide array of structures.

IDPs are especially useful for biomedical purposes because they can undergo phase transitions – changing from a liquid to a gel, for example, or a soluble to an insoluble state, and back again – in response to environmental triggers, like changes in temperature. This ability has made IDPs a go-to tool for long-term drug delivery, as IDPs can be injected in liquid form into the body and then solidify into a gel that slowly releases medication.

But while their flexible structure makes IDPs useful in a variety of applications, researchers previously thought that this flexibility limited the stability of the resulting materials.

In a 2015 paper in Nature Materials, Ashutosh Chilkoti, the chair of Duke Biomedical Engineering, and Felipe Garcia Quiroz, a PhD graduate of the Chilkoti Lab who is now a postdoctoral fellow at Rockefeller University, demonstrated that they could precisely tune the stability of IDP-based materials by controlling how quickly IDPs associate and dissociate in response to environmental cues.

"Unlike well-folded proteins, conventional IDPs have a hard time shielding different parts of their structures from each other," Quiroz said. "So as IDPs become more abundant in a solution they begin to collide and clash frequently, with some of their exposed structures weakly sticking together and rapidly breaking apart."

If the rate of association and dissociation is equal, the IDP is in equilibrium and it doesn't undergo any behavior change. But if something in the environment changes, such as temperature, then segments of the IDPs stick together for longer periods of time and break apart with less frequency, resulting in a phase transition from a soluble to an insoluble state that can be harnessed to build materials.

Upon removing the environmental stimulus, however, conventional IDPs go back to exhibiting very weak associations, and the previously assembled materials fall apart.

In their new work, Chilkoti and Quiroz created materials using newly designed IDPs that change phase at different temperatures, and demonstrated that upon phase separation these IDPs are knocked out of their usual equilibrium behavior. This triggers a process known as hysteresis, in which IDPs will stick together even if the environmental trigger of the initial phase transition is removed.

"What is exciting about our new work is that we've shown that we can dial the degree of hysteresis to identify designs in which these proteins will stick together readily, and once those associations emerge, it becomes very difficult to break them," Quiroz said. "IDPs are typically thought as being weakly sticky, but we now show that it's possible to design super sticky IDPs, which become very stable building blocks.

"That super stickiness only emerges after we apply an environmental trigger, so they otherwise behave as regular IDPs and we don't have to worry about their stickiness as we handle them. From a materials perspective, many of our favorite materials are those that are easy to prepare, but can rapidly mature to a state that is highly stable and difficult to disrupt. Cement is a great example of this."

By showing that they could make a highly stable material out of IDPs, Quiroz said, they could build on earlier work with IDPs in fields like regenerative medicine. For example, in their liquid form, IDPs can flow into a wound cavity, adopt its shape and then phase into a gel to provide structural support and recruit key cells for tissue repair.

Because current IDP-based materials lack stability, their effect is usually short-lived, as the materials erode fairly quickly, but this new approach could make IDPs a good source of stable materials for wound-healing.

"IDPs have had a set of known characteristics, and we have been working within that range of characteristics to explore potential biomedical applications for the last two decades," Quiroz said. "But now we essentially have new tools to play with, and that allows us to be more creative. Our discovery adds complexity to what we are able to do with IDP-based materials for applications spanning materials science and biology, which is exciting."

This story is adapted from material from Duke University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.