SGL Group has announced the sale of SGL Rotec GmbH & Co KG, a manufacturer of composite blades for wind turbines.

Glass-fibre reinforced PBT solves flame retardancy problem on French railways

French company ABB in Lyon has selected polybutylene terephthalate (PBT) Ultradur® B4450 G5 from BASF for its DC contactors for use on railways.

Quickstep Holdings Ltd has signed a US$75 million deal with aerospace group Lockheed Martin to supply 120 sets of carbon composite wing flaps for the C-130

Chinese fibreglass producer Jushi is opening a new plant in Egypt.