French fiber specialist Chomarat has received DNV GL certification for its range of glass and carbon multiaxial reinforcements for the marine market.

The reinforcements are available under the brand names G-PlyTM and C-PlyTM.

‘By developing innovative reinforcements made from fiber glass or carbon, we can improve the performance of composite parts and meet the specific demands of the marine market – reduced weight, improved surface finish and better resin flow,’ said Vincent Cholvy, marine market manager. ‘Chomarat is a leader in the marine reinforcements market. Our DNV GL certification confirms this expertise and proves that we are now ready to conquer new markets requiring this qualification.’

This story uses material from Chomarat with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.