The polyamide grades reportedly have reduced warping and curling, and improved mechanical properties.
The polyamide grades reportedly have reduced warping and curling, and improved mechanical properties.

Spain-based MyMat Solutions has launched a new range of nylon filaments for the 3d printing of nylon.

Ultra nylon and Soft Nylon polyamide grades reportedly have reduced warping and curling, and improved mechanical properties.

Ultra Nylon also has high mechanical strength and high temperature and is suitable for automotive, drone and industrial applications. Its formulation introduces carbon fiber.

Soft Nylon reportedly has wear resistance, flexible, smooth and improved aesthetics.

The company is also publishing a free guide to 3d printing product design, available from the company website.