As part of the partnership, Xenia will develop products based on long andshort carbon fiber reinforced thermoplastic composites for the European market.
As part of the partnership, Xenia will develop products based on long andshort carbon fiber reinforced thermoplastic composites for the European market.

As part of the partnership, Xenia will develop products based on PlastiComp’s Complet long carbon fiber reinforced thermoplastic composites and Xenia’s XECARB short carbon fiber reinforced thermoplastic composites for the European market.

‘We are delighted to expand our capabilities with carbon fiber technology through our partnership with PlastiComp,’ said Xenia president Fabio Azzolin. ‘Xenia now has a full line of carbon fiber composites that will allow us to develop more applications benefitting from the reduced weight and high-performance properties provided by carbon fiber reinforced materials.’

Wear reduction

Injection moldable Complet long fiber composite pellets from PlastiComp are available with 15-50% carbon fiber in thermoplastic polymers from polypropylene to PEEK. Composite formulations can be custom engineered to include wear reduction, electrical conductivity, and flame retardant functions in addition to long fiber structural reinforcement. Continuous fiber reinforced tapes are available in 0.5 to 7.5 cm widths in the same polymer range as pellet products.

PlastiComp recently developed a line of hybrid long glass and carbon fiber composites that combine long glass and carbon fiber together into a single ready-to-mold pellet. Hybrid products are available with variable combinations of the fiber types to bridge the performance gap between using either of these two fibers alone.

Xenia engineers and manufactures reinforced thermoplastic composites for structural applications used in the most advanced fields. It combines reinforcing fibers, such as carbon or aramid, with functional additives, such as PTFE, to improve the mechanical and tribological properties of thermoplastic polymers.

Metal replacement

Xenia compounds fiber reinforcement with thermoplastic elastomers for applications where flexibility, resistance to fatigue, and impact are required or with stiffer engineering thermoplastic polymers, such as PA, PPS, PPA, or PEEK, for heavy duty, high-performance, and high temperature environments. Their products are highly recommended for the replacement of metals in applications ranging from industrial, transportation, oil and gas, agriculture, to technical sports.