Xenia Materials combines carbon fibre with thermoplastics such as polyamide (PA) 66, PA 12, and PA 11.
Xenia Materials combines carbon fibre with thermoplastics such as polyamide (PA) 66, PA 12, and PA 11.

The Xecarb range is made up of three product lines:

  • STRONG, which combines a variety of base polymers with 30% carbon fibre;
  • DOUBLE STRONG in which the polymers are reinforced with 50% carbon fibre and where tensile modulus values can reach 32,000 MPa; and
  • LOW WEAR, which contains 30% carbon fibre and 20% PTFE, for applications requiring a low friction coefficient, self-lubrication,or wear resistance (e.g. sliding guides and bearings).

Xenia Materials is located near Vicenza in Italy.