The HZRDUS Smoke Black RDX, made by True Temper Sports, incorporates the company’s new HexTow HM54 carbon fiber.
The HZRDUS Smoke Black RDX, made by True Temper Sports, incorporates the company’s new HexTow HM54 carbon fiber.

Hexcel has supplied its carbon fiber material to make a new range of golf shafts.

The HZRDUS Smoke Black RDX, made by True Temper Sports, incorporates the company’s new HexTow HM54 carbon fiber, which is suitable for recreational applications, Hexcel says. It also includes the high tensile strength HexTow IM2C carbon fiber to build into the HZRDUS shafts.

Tom Haulik, Sales Director – Global Fibers at Hexcel said, ‘True Temper has a heritage of being the worldwide leader in the manufacturing of golf shafts, so we are very excited to see our new HexTow HM54 fibers used in their latest HZRDUS shaft. HexTow HM54 is the perfect application for a high-performance golf shaft such as HZRDUS Smoke RDX.’

This story uses material from Hexcel, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.