The RP542-4 system has reportedly been designed as an intermediately toughened system following the launch of the company’s RP542-1 and RP549 systems.
The RP542-4 system has reportedly been designed as an intermediately toughened system following the launch of the company’s RP542-1 and RP549 systems.

PRF Composite Materials has developed a new prepreg for use with unidirectional (UD) and woven carbon fabrics.

The RP542-4 system has reportedly been designed as an intermediately toughened system following the launch of the company’s RP542-1 and RP549 systems.

‘The mechanical testing carried out shows the system to have excellent tensile, compressive, flexural and interlaminar properties and a relatively high Tg of 138°C after curing at 120°C,’ said head of technology, Heather Hughes. ‘The onset Tg can be improved by 20°C to 120°C after post curing at 140°C for 2 hours. Adding to its usability, the system also has an out life of 60 days at 20°C.’

The system is available on 300 gsm and 600 gsm unidirectional carbon and PRF’s range of fabrics in a variety of fiber types, the company says.

This story uses material from PRF, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.