Scientists have created self-assembled monolayers that are stable in air, made from spherical buckyballs with 'tails' of of ethylene glycol.

A newly synthesized class of ‘super-diamond’ carbon-based material can alter its properties depending on which guest atoms are trapped in its cages.

A nanoparticle comprising tiny spheres of copper dotted with single atoms of ruthenium makes an effective light-powered catalyst for producing syngas.

For the first time, researchers have been able to grow, image with atomic resolution and investigate the properties of 2D amorphous carbon.

Researchers have developed a new version of the high-pressure carbon monoxide gas-phase process for producing single-walled carbon nanotubes.

Turning natural atomic flaws inside diamond anvils into quantum sensors offers a novel way to study the effects of pressure on materials.

Taking inspiration from drug discovery, scientists have developed metal-organic frameworks that can capture carbon dioxide from wet flue gasses.