The carbon nanotube dough can be transformed into arbitrary shapes defined by a mold. Photo: Jiaxing Huang Group, Northwestern University.Northwestern University's Jiaxing Huang is ready to reignite carbon nanotube research. And he's doing so with a common chemical that was once used in household cleaners.
Using an inexpensive, already mass produced, simple solvent called cresol, Huang has discovered a way to produce disperse carbon nanotubes at unprecedentedly high concentrations without the need for additives or harsh chemical reactions to modify the nanotubes. In a surprising twist, Huang also found that as the nanotubes' concentrations increase, the material transitions from a dilute dispersion to a thick paste, then a free-standing gel and finally a kneadable dough that can be shaped and molded. These findings are reported in a paper in the Proceedings of the National Academy of Sciences.
"Because of their exceptional mechanical, thermal and electrical properties, carbon nanotubes have attracted a lot of attention for a number of applications," said Huang, professor of materials science and engineering in Northwestern's McCormick School of Engineering. "But after decades of research and development, some of the excitement has faded."
The reason? Carbon nanotubes are notoriously tricky to process – especially in large quantities. About 10,000 times thinner than a human hair, the wiry, tube-shaped structures are said to be stronger than steel and to conduct heat and electricity far better than copper. But when mass produced – usually in the form of powders – the tubes twist and clump together, which is a major barrier to the material's widespread applications.
"Aggregated tubes are hard to disperse in solvents," Huang explained. "And if you cannot get a good dispersion, then you won't be able to make high-quality nanotube thin films that many applications rely on."
In order to overcome this problem, previous researchers coated the nanotubes with additives, which chemically altered their surfaces and forced them to separate. Although these methods do work, they leave behind residues or alter the nanotubes' surface structures, which can blunt their desirable properties.
By contrast, Huang's team found that cresol does not deteriorate the carbon nanotubes' surface functions. And, after separating the entangled tubes, the researchers could remove the chemical by simply washing it off or heating it until it evaporates.
After unlocking a new way to make carbon nanotubes in higher and higher concentrations, Huang and his team also discovered new forms of the material. As the concentration of carbon nanotubes increases, the material transitions from a dilute dispersion to a spreadable paste to a free-standing gel and finally to a kneadable dough. These various forms can be molded, reshaped or used as conductive ink for 3D printing.
"The dough state of nanotubes is fascinating," said Kevin Chiou, a graduate student in Huang's laboratory and first author of the paper. "It can be readily shaped and molded into arbitrary structures just like playdough."
"Essentially, this solvent system now makes nanotubes behave just like polymers," Huang said. "It is really exciting to see cresol-based solvents make once hard-to-process carbon nanotubes as usable as common plastics."
This story is adapted from material from Northwestern University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.