"Graphene is very strong, but it can break suddenly. We found that graphene oxide, however, will deform first before eventually breaking."Horacio Espinosa, Northwestern's McCormick School of Engineering
Since its discovery, graphene has captured the attention of scientists and engineers for its many extraordinary properties. But graphene oxide – an oxidized derivative of graphene – has largely been viewed as graphene's inferior cousin.
"Graphene is so perfect," said Northwestern Engineering's Jiaxing Huang. "And graphene oxide is more defective, so it's like the weaker, less exciting version of graphene."
Now a Northwestern University team has found that graphene oxide's seemingly undesirable defects surprisingly give rise to exciting mechanical properties. Led by Horacio Espinosa, professor in manufacturing and entrepreneurship at Northwestern's McCormick School of Engineering, the researchers used a unique experimentation and modeling approach to become the first to examine the mechanics of this previously ignored material at the atomic level. What they discovered could potentially unlock the secret to successfully scaling up production of graphene oxide.
"Our team discovered that graphene oxide exhibits remarkable plastic deformation before breaking," said Espinosa. "Graphene is very strong, but it can break suddenly. We found that graphene oxide, however, will deform first before eventually breaking."
Huang compares the difference in the materials' properties to common objects. "Ceramic is strong," he says, "but if you break it, it will shatter. Now if a plastic cup is squeezed, it will bend before it snaps."
Supported by the Army Research Office and the National Science Foundation's Designing Materials to Revolutionize and Engineer Our Future program, the research is described in Nature Communications. In addition to Espinosa, Northwestern Engineering's Jiaxing Huang, associate professor of materials science and engineering, and SonBinh Nguyen, professor of chemistry in the Weinberg College of Arts and Sciences, are co-principal investigators on the project. Postdoctoral fellow Xiaoding Wei and graduate students Rafael Soler-Crespo and Lily Mao are co-first authors of the paper.
The team found that graphene oxide's plasticity is due to an unusual mechanochemical reaction. In graphene oxide, two carbon atoms bind with a single oxygen atom, a formation known as an epoxide. This can be imagined as a triangle with two carbon atoms at the base and an oxygen atom at the top. When an epoxide's bonds are chemically broken, the carbon-oxygen bonds break first, leaving the carbon-carbon bond intact. In contrast, the research team found that when a mechanical force is applied to graphene oxide, the carbon-carbon bond breaks first, leaving the carbon-oxygen bonds in place.
"We uncovered this surprise on the atomic scale," Nguyen said. "This is completely different than what occurs in other materials and a very unusual property for the graphene oxide sheet."
Knowing how graphene oxide functions at the atomic scale could allow researchers to tune the material's properties. The Northwestern team is now extending its research to understanding the mechanical properties of graphene oxide-polymer interfaces, which is critical to scaling up the material.
"Our studies imply that the answers to scaling up graphene oxide may lie, in part, to the chemistry at the atomic level," Espinosa said. "With more information obtained at different length scales as well as advances in synthesis methods, we will eventually piece the puzzle together."
This story is adapted from material from Northwestern University's McCormick School of Engineering, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.