This scanning tunneling microscopy image shows a graphene nanoribbon that was made bottom-up from a molecular precursor. Image: Oak Ridge National Laboratory, US Department of Energy; scanning tunneling microscopy by Chuanxu Ma and An-Ping Li.A new way to grow narrow ribbons of graphene, a lightweight and strong structure of single-atom-thick carbon atoms linked into hexagons, may address a shortcoming that has prevented the material from achieving its full potential in electronic applications. Graphene nanoribbons, mere billionths of a meter wide, exhibit different electronic properties than two-dimensional sheets of the material.
"Confinement changes graphene's behavior," said An-Ping Li, a physicist at the US Department of Energy's Oak Ridge National Laboratory (ORNL). While graphene in sheets is an excellent electrical conductor, narrowing graphene can turn the material into a semiconductor if the ribbons are made with a specific edge shape. However, previous efforts to make graphene nanoribbons employed a metal substrate that hindered the ribbons' useful electronic properties.
Now, scientists at ORNL and North Carolina State University report in a paper in Nature Communications being the first to grow graphene nanoribbons without a metal substrate. Instead, they injected charge carriers able to promote a chemical reaction that converts a polymer precursor into a graphene nanoribbon. At selected sites, this new technique can create interfaces between materials with different electronic properties. Such interfaces are the basis of semiconductor electronic devices, from integrated circuits and transistors to light-emitting diodes and solar cells.
"Graphene is wonderful, but it has limits," said Li. "In wide sheets, it doesn't have an energy gap – an energy range in a solid where no electronic states can exist. That means you cannot turn it on or off." When a voltage is applied to a sheet of graphene in a device, electrons flow freely as they do in metals, severely limiting graphene's application in digital electronics.
"When graphene becomes very narrow, it creates an energy gap," Li explained. "The narrower the ribbon is, the wider is the energy gap."
In very narrow graphene nanoribbons, with a width of a nanometer or even less, how structures terminate at the edge of the ribbon is important too. For example, cutting graphene along the side of a hexagon creates an edge that resembles an armchair; this material can act like a semiconductor. Excising triangles from graphene creates a zigzag edge – and a material with metallic behavior.
To grow graphene nanoribbons with a controlled width and edge structure from polymer precursors, previous researchers had used a metal substrate to catalyze the chemical reaction. However, the metal substrate suppresses useful edge states and shrinks the desired band gap.
Li and colleagues set out to get rid of this troublesome metal substrate. At the Center for Nanophase Materials Sciences, a DOE Office of Science User Facility at ORNL, they used the tip of a scanning tunneling microscope to inject either negative charge carriers (electrons) or positive charge carriers (‘holes’) to try to trigger the key chemical reaction. This revealed that only holes could trigger the reaction. They were subsequently able to make a ribbon that was only seven carbon atoms wide – less than one nanometer – with edges in the armchair conformation.
"We figured out the fundamental mechanism, that is, how charge injection can lower the reaction barrier to promote this chemical reaction," Li said. Moving the tip along the polymer chain, the researchers could select where they triggered this reaction and convert one hexagon of the graphene lattice at a time.
Next, the researchers will make heterojunctions with different precursor molecules and explore functionalities. They are also eager to see how long electrons can travel in these ribbons before scattering, and will compare them with a graphene nanoribbon made another way and known to conduct electrons extremely well. Using electrons like photons could provide the basis for a new electronic device that could carry current with virtually no resistance, even at room temperature.
"It's a way to tailor physical properties for energy applications," Li said. "This is an excellent example of direct writing. You can direct the transformation process at the molecular or atomic level." Plus, the process could be scaled up and automated.