This scanning electron microscope image shows two traces of laser-induced graphene on a polyimide film. A laser mounted to the microscope was used to burn the patterns into the film. Image: Tour Group/Rice University.You don't need a big laser to make laser-induced graphene (LIG). Scientists at Rice University, the University of Tennessee, Knoxville (UT Knoxville) and Oak Ridge National Laboratory (ORNL) are using a very small visible beam to burn the foamy form of carbon into microscopic patterns.
The labs of Rice chemist James Tour, which discovered the original method for turning a common polymer into graphene in 2014, and Tennessee/ORNL materials scientist Philip Rack revealed that they can now watch the conductive material form by making small traces of LIG in a scanning electron microscope (SEM).
The altered process, reported in a paper in ACS Applied Materials & Interfaces, creates LIG with features more than 60% smaller than the macro version and almost 10 times smaller than typically achieved with the former infrared laser. Lower-powered lasers also make the process less expensive, Tour said, which could lead to wider commercial production of flexible electronics and sensors.
"A key for electronics applications is to make smaller structures so that one could have a higher density, or more devices per unit area," Tour said. "This method allows us to make structures that are 10 times denser than we formerly made."
To prove the concept, the lab made flexible humidity sensors that are invisible to the naked eye and directly fabricated on polyimide, a commercial polymer. The devices were able to sense human breath with a response time of 250 milliseconds.
"This is much faster than the sampling rate for most commercial humidity sensors and enables the monitoring of rapid local humidity changes that can be caused by breathing," said the paper's lead author, Rice postdoctoral researcher Michael Stanford.
The smaller lasers pump light at a wavelength of 405nm, in the blue-violet part of the spectrum. These are less powerful than the industrial lasers used by the Tour group and others around the world to burn graphene into plastic, paper, wood and even food. The SEM-mounted laser burns only the top 5µm of the polymer, writing graphene features as small as 12µm.
Working directly with ORNL let Stanford capitalize on the national lab's advanced equipment. "That's what made this joint effort possible," Tour said.
"I did a lot of my PhD research at ORNL, so I was aware of the excellent facilities and scientists and how they could help us with our project," Stanford said. "The LIG features we were creating were so small that they would have been next-to-impossible to find if we were to lase the patterns and then search for them in the microscope later."
Tour, whose group recently introduced flash graphene to instantly turn trash and food waste into the valuable material, said the new LIG process offers a novel path toward writing electronic circuits into flexible substrates like clothing. "While the flash process will produce tons of graphene, the LIG process will allow graphene to be directly synthesized for precise electronics applications on surfaces," Tour said.
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.