This transmission electron microscope image shows the interlayer spacing of turbostratic graphene produced at Rice University by flashing carbon black from discarded rubber tires with a jolt of electricity. Image: Tour Research Group/Rice University.Scientists at Rice University have optimized a process for converting waste from rubber tires into graphene that can, in turn, be used to strengthen concrete.
According to chemist James Tour, the environmental benefits of adding graphene to concrete are clear. "Concrete is the most-produced material in the world, and simply making it produces as much as 9% of the world's carbon dioxide emissions. If we can use less concrete in our roads, buildings and bridges, we can eliminate some of the emissions at the very start."
Recycled tire waste is already used as a component of Portland cement, but graphene has been proven to strengthen cementitious materials, concrete among them, at the molecular level.
While the majority of the 800 million tires discarded annually are burned for fuel or ground up for other applications, 16% of them wind up in landfills. "Reclaiming even a fraction of those as graphene will keep millions of tires from reaching landfills," Tour said.
The 'flash' process introduced by Tour and his colleagues in 2020 has been used to convert food waste, plastic and other carbon sources into graphene by exposing them to a jolt of electricity that removes everything but carbon atoms from the sample (see New process turns plastic into graphene in a flash). Those atoms reassemble into valuable turbostratic graphene, which has misaligned layers that are more soluble than the graphene produced via exfoliation from graphite. That makes it easier to use in composite materials.
Rubber proved more challenging than food or plastic to turn into graphene, but the lab optimized the process by using commercial pyrolyzed waste rubber from tires. After useful oils are extracted from waste tires, this carbon residue, known as carbon black, has until now had near-zero value, Tour said.
Tire-derived carbon black or a blend of shredded rubber tires and commercial carbon black can be flashed into graphene. Because the resulting turbostratic graphene is soluble, it can easily be added to cement to make more environmentally friendly concrete. This research, led by Tour and Rouzbeh Shahsavari of C-Crete Technologies, is reported in a paper in Carbon.
The Rice lab flashed tire-derived carbon black and found that about 70% of the material converted to graphene. When flashing shredded rubber tires mixed with plain carbon black to add conductivity, about 47% were converted to graphene. Elements besides carbon were vented out for other uses.
The electrical pulses lasted between 300 milliseconds and 1 second. The lab calculated electricity used in the conversion process would cost about $100 per ton of starting carbon.
The researchers then blended minute amounts of tire-derived graphene – 0.1 weight/percent (wt%) for tire carbon black and 0.05 wt% for carbon black and shredded tires – with Portland cement and used it to produce concrete cylinders. Tested after curing for seven days, the cylinders showed gains of 30% or more in compressive strength.
"This increase in strength is in part due to a seeding effect of 2D graphene for better growth of cement hydrate products, and in part due to a reinforcing effect at later stages," Shahsavari explained.
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.