Researchers have found that reducing the repulsive interactions between electrons in magic-angle graphene makes its superconductivity more robust.

Machine learning proves itself for CNT composites

machine learning algorithm trained to predict pullout forces of carbon nanotubes from polymer matrix

graphene oxide can affect the response of synapses in the brain potentially leading to treatment for PTSD

Researchers have discovered that the electronic properties of halide perovskites hinge on the way their atomic lattice twists and turns.

novel bio-polymer based on microalgae could offer a sustainable alternative to synthetic polymers produced from fossil fuels

Using optical spectroscopy, researchers have shown that the insulating behavior of 'bad metals' can be explained with conventional theories.

Scientists have combined two cutting-edge analytical techniques to achieve nanoscale mapping of each distinct electronic phase in nickelates.

Researchers used ultrafast nanometric imaging to show, for the first time, that populations of carbon dots contain both good and bad emitters.

By using 'scientific machine learning', researchers have gained a better understanding of how lithium ions more in and out of battery electrodes.

imperfections in the highly regular crystal structure of diamond could hold the key for ultrasensitive biosensing

Using X-rays, researchers have revealed the presence of both lithium hydride and lithium fluoride in the interphase of lithium-metal batteries.

Using advanced electron microscopes, researchers have imaged the boundary between 2D and 3D materials, and correlated it with their properties.

Using a weakly binding electrolyte, researchers developed a lithium-metal battery that can be repeatedly recharged at temperatures as low as -60°C.

Researchers have discovered a halide ion conductor that could dramatically improve the efficiency and lifespan of solid-state sodium-ion batteries.

An exotic metallic material made of cerium, bismuth and palladium can produce a giant Hall effect in the total absence of any magnetic field.

porous silica nanoparticles impregnated with nanoceria offer novel way to treat osteoporosis

By fabricating raised squares on the surface of an antiferromagnetic crystal, researchers have developed a novel data storage medium.

News archive…

Connect with us
Most viewed in characterization…
News
 

thin films of zirconium oxide could enable a next generation of low-voltage and -power nonvolatile memory and other nanoscale devices

Current research
 

News
 

Synthetic vascular grafts improved by seaweed molecule

Current research
 

Current research