Researchers employed a set of advanced characterization tools to study the atomic structure evolution of a state-of-the art OER electrocatalyst, strontium iridate (SrIrO3), in acid electrolyte. Image: Zhenxing Feng, Oregon State University. Efficiently mass-producing hydrogen from water is closer to becoming a reality thanks to researchers at Oregon State University (OSU), Cornell University and the Argonne National Laboratory. Using advanced experimental tools, these researchers were able to forge a clearer understanding of an electrochemical catalytic process that's cleaner and more sustainable than deriving hydrogen from natural gas. They report their findings in a paper in Science Advances .
Hydrogen is found in a wide range of compounds on Earth, most commonly combining with oxygen to make water, and it has many scientific, industrial and energy-related roles. It also occurs in the form of hydrocarbons, compounds consisting of hydrogen and carbon such as methane, the primary component of natural gas.
"The production of hydrogen is important for many aspects of our life, such as fuel cells for cars and the manufacture of many useful chemicals such as ammonia," said OSU's Zhenxing Feng, a chemical engineering professor who led the study. "It's also used in the refining of metals, for producing man-made materials such as plastics and for a range of other purposes."
According to the US Department of Energy, the US currently produces most of its hydrogen from a methane source such as natural gas via a technique known as steam-methane reforming. This process involves subjecting methane to pressurized steam in the presence of a catalyst, creating a reaction that produces hydrogen and carbon monoxide, as well as a small amount of carbon dioxide.
The next step is referred to as the water-gas shift reaction, in which the carbon monoxide and steam are reacted via a different catalysis to produce carbon dioxide and additional hydrogen. In the last step, pressure-swing adsorption, carbon dioxide and other impurities are removed, leaving behind pure hydrogen.
"Compared to natural gas reforming, the use of electricity from renewable sources to split water for hydrogen is cleaner and more sustainable," Feng said. "However, the efficiency of water-splitting is low, mainly due to the high overpotential – the difference between the actual potential and the theoretical potential of an electrochemical reaction – of one key half-reaction in the process, the oxygen evolution reaction, or OER."
A half-reaction is either of the two parts of a redox, or reduction-oxidation, reaction, in which electrons are transferred between two reactants; reduction refers to gaining electrons, oxidation means losing electrons. The concept of half-reactions is often used to describe what goes on in an electrochemical cell, and half-reactions are commonly used as a way to balance redox reactions. Overpotential is the margin between the theoretical voltage and the actual voltage necessary to cause electrolysis, which is a chemical reaction driven by the application of electric current.
"Electrocatalysts are critical to promoting the water-splitting reaction by lowering the overpotential, but developing high-performance electrocatalysts is far from straightforward," Feng said. "One of the major hurdles is the lack of information regarding the evolving structure of the electrocatalysts during the electrochemical operations. Understanding the structural and chemical evolution of the electrocatalyst during the OER is essential to developing high-quality electrocatalyst materials and, in turn, energy sustainability."
Feng and his collaborators used a set of advanced characterization tools to study the atomic structural evolution of a state-of-the art OER electrocatalyst – strontium iridate (SrIrO3 ) – in an acid electrolyte.
"We wanted to understand the origin of its record-high activity for the OER – 1000 times higher than the common commercial catalyst, iridium oxide," Feng explained. "Using synchrotron-based X-ray facilities at Argonne and lab-based X-ray photoelectron spectroscopy at the Northwest Nanotechnology Infrastructure site at OSU, we observed the surface chemical and crystalline-to-amorphous transformation of SrIrO3 during the OER."
These observations led to a deeper understanding of what was going on behind strontium iridate's ability to work so well as a catalyst. "Our detailed, atomic-scale finding explains how the active strontium iridate layer forms on strontium iridate and points to the critical role of the lattice oxygen activation and coupled ionic diffusion on the formation of the active OER units," Feng said.
He added that the work provides insight into how applied potential facilitates the formation of the functional amorphous layers at the electrochemical interface and leads to possibilities for the design of better catalysts.
This story is adapted from material from Oregon State University , with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source .