Studies with the quantum sensor showed that bismuth ferrite exhibits spiral magnetic ordering, with two superimposed electron spins (shown in red and blue in the image) adopting opposing orientations and rotating in space. Image: Universität Basel, Departement Physik.
Studies with the quantum sensor showed that bismuth ferrite exhibits spiral magnetic ordering, with two superimposed electron spins (shown in red and blue in the image) adopting opposing orientations and rotating in space. Image: Universität Basel, Departement Physik.

For the first time, physicists have successfully imaged spiral magnetic ordering in a multiferroic material. These materials are considered highly promising candidates for future data storage media.

The physicists were able to prove their findings using unique quantum sensors developed at Basel University that can analyze electromagnetic fields on the nanometer scale. The results – obtained by scientists from the University of Basel's Department of Physics, the Swiss Nanoscience Institute, and the University of Montpellier and several laboratories from University Paris-Saclay, both in France – were recently reported in a paper in Nature.

Multiferroics are materials that simultaneously react to electric and magnetic fields. These two properties are rarely found together, and their combined effect makes it possible to change the magnetic ordering of materials using electric fields.

This offers particular potential for novel data storage devices: multiferroic materials can be used to create nanoscale magnetic storage media that can be deciphered and modified using electric fields. Magnetic media of this kind would consume very little power and operate at very high speeds. They could also be used in spintronics – a new form of electronics that uses electrons' spin as well as electrical charge.

Bismuth ferrite is a multiferroic material that exhibits electric and magnetic properties even at room temperature. While its electrical properties have been studied in depth, there was no suitable method for representing magnetic ordering on the nanometer scale until now.

The group, led by Patrick Maletinsky from the Swiss Nanoscience Institute and the University of Basel's Department of Physics, has developed quantum sensors based on diamonds with nitrogen vacancy centers. In collaboration with colleagues at the University of Montpellier and the University Paris-Saclay, they were able to use these quantum sensors to depict and study the magnetic ordering of a thin bismuth ferrite film for the first time. Knowing how the electron spins behave and how the magnetic field is ordered is of crucial importance for the future application of multiferroic materials in data storage.

The scientists were able to show that bismuth ferrite exhibits spiral magnetic ordering, with two superimposed electron spins adopting opposing orientations and rotating in space, whereas it was previously assumed that this rotation took place within a plane. According to the researchers, the quantum sensors now show that a slight tilt in these opposing spins leads to spatial rotation with a slight twist.

"Our diamond quantum sensors allow not only qualitative but also quantitative analysis. This meant we were able to obtain a detailed picture of the spin configuration in multiferroics for the first time," explains Maletinsky. "We are confident that this will pave the way for advances in research into these promising materials."

The quantum sensors they used consist of two tiny monocrystalline diamonds, whose crystal lattices have a vacancy and a nitrogen atom in two neighboring positions. These nitrogen vacancy centers contain orbiting electrons whose spins respond very sensitively to external electric and magnetic fields, allowing the fields to be imaged at a resolution of just a few nanometers.

Scientists at the University of Montpellier took the magnetic measurements using the quantum sensors produced in Basel. The samples were supplied by experts from the CNRS/Thales laboratory at University Paris-Saclay, who are leading lights in the field of bismuth ferrite research.

The quantum sensors used in the research are suitable for studying a wide range of other materials, as they provide precisely detailed qualitative and quantitative data both at room temperature and at temperatures close to absolute zero. In order to make them available to other research groups, Patrick Maletinsky founded a start-up called Qnami in 2016 in collaboration with Mathieu Munsch. Qnami produces the diamond sensors and provides application advice to its customers from academia and industry.

This story is adapted from material from the University of Basel, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.