Core Molding Technologies Inc, a molder of glass fiber reinforced plastics, has acquired substantially all of the assets of CPI Binani Inc (CPI), located i
Check out the stories that were most popular with our readers last week.
Volkswagen AG’s Porsche division plans to buy a 25% stake in Capricorn Composite GmbH, a German auto-parts and carbon fiber producer, according to Bloomber
Hexion Inc has developed a coil spring made of plastic composite in cooperation with Sogefi for Audi.
QA1 has developed a line of carbon fiber driveshafts for vehicles with up to 500 horsepower/pound-foot of torque.
DolphiTech says that its DolphiCam Ultrasound NDT Camera System has received new functionality for drilled hole inspections on carbon fiber reinforced plas
Holding Company Composite has started a new large scale carbon fiber production line developed for industrial grade carbon fiber.
Owens Corning has launched a number of new glass fiber materials at JEC.
NetComposites has developed injection mouldable long fiber thermoplastic (LFT) Flax/PP and Jute/PP pellets.
Johns Manville has developed two new products, a multi-end roving for sheet moulding compound (SMC) and chopped strand glass fiber for high-performance pol
Austrian hybrid parts specialist Teufelberger has installed a lightweight carbon fiber reinforced plastic component for the particle accelerator at the CER
Common Fibers, a small startup company in the US, has developed new technology that can create a hinge directly in a sheet of carbon fiber by using a laser
The first ever approval of a structural composite part for a commercial ship was announced at the E-LASS (European network for lightweight applications at
Discover the stories that were most popular with our readers last week.