The transportation of the GloBlade wind turbine blade prototypes is thought to be the longest cargo ever to have been transported by air, according to LM Wind Power.

"The new blade type will help the wind farm developers take wind energy to new heights. These blades ensure reliable, clean electricity in lower wind areas for turbines at 1.5-1.7 MW," says Frank V. Nielsen, Chief Technology Officer.