Aguz Marine produces motorboats based on designs developed by Ferragni Tollini & Yacht Design.
Aguz Marine produces motorboats based on designs developed by Ferragni Tollini & Yacht Design.

Aguz Marine was established in 2010 to produce motorboats of 26-50 ft, based on designs developed by Ferragni & Tollini Yacht Design.

The first design will be the Aguz Open Line 36 and the first boat will go into the water in early April. This boat has two or three cabins and two engines, and accommodates up to 10 people. The hull is manufactured in vinyl ester composite using the infusion process.

Aguz Marine is planning to manufacture two watercraft per month and intends to include three other projects acquired from Ferragni & Tollini in its portfolio: the 26, 42 and 50 ft motorboats.