Polynt Composites Europe says that it has completed its range of gel coats developed specifically for the swimming pool market.

The gel coats are available in a range of colours and have improved resistance to osmosis and reduced colour fade caused by sunlight or chlorinated water treatment chemicals. The gel coats come ready to apply, in both brush and spray with the addition of methyl ethyl ketone peroxide (MEKP) and the spray grade is for use with airless or air assisted spray equipment.