As the infrastructure ages and mass transit platforms are repaired and replaced, concrete decks are being upgraded with lightweight, corrosion resistant pultuded decks.
As the infrastructure ages and mass transit platforms are repaired and replaced, concrete decks are being upgraded with lightweight, corrosion resistant pultuded decks.

Applications for the GR250 pultruded deck include:

  • mass transit platforms;
  • decking for walkways and platforms;
  • marina dock decking;
  • pedestrian bridge decks; and 
  • commercial piers.

The pultruded deck was designed for rapid construction with an integrated tactile and ADA compliant wearing surface. A unique connection system allows contractors to install the deck in a fraction of the time of a concrete deck with all of the benefits of corrosion resistance, light weight and reduced maintenance.

Creative Pultrusions Inc (CPI) is based in Alum Bank, Pennsylvania, USA, and is owned by UK headquartered Hill & Smith Holdings PLC (HS).