Corecell has been developed for applications where PVC and balsa are commonly used.
Corecell has been developed for applications where PVC and balsa are commonly used.

WINDPOWER 2011 takes place on 22-25 May in Anaheim, organised by the American Wind Energy Association (AWEA).

Gurit will be highlighting its RENUVO Blade Repair system and its extended core material offering for the wind energy market, which now comprises:

  • Corecell™ T-Foam, a SAN based core material with low resin uptake;
  • G-PET recyclable thermoplastic foam with a good balance of mechanical properties, temperature resistance, density and cost;
  • PVCell™ G-Foam, a closed cell, crosslinked PVC foam developed specifically for the Chinese wind energy market; and
  • Balsaflex® balsa wood.