The ‘Modular Fabrication’ stand was designed by Ben van Berkel of Dutch architectural design firm UNStudio, and engineered, manufactured and installed by Premier Composite Technologies (PCT), a Dubai-based supplier of lightweight architectural components manufactured using composites.

The stand design is based on the repetition of a single geometric module. It was moulded from carbon fibre and epoxy resin combined with a structural foam core.

PCT used the 5 m x 10 m stand at the 100% Design in London on 22-25 September, a contemporary design show attracting interior designers, architects, retailers and specifiers.