The 41 m (135 ft) Majesty 135 is the largest Majesty Yacht ever built by United Arab Emirates based Gulf Craft.

The boat was built to order with the emphasis on comfort. The construction incorporated SP-High Modulus’ Corecell M-Foam core material, which was chosen because of its high temperature tolerance, no outgassing, high elongation and toughness and its Bureau Veritas (BV) and Registro Italiano Navale (RINA) approvals.

SP-High Modulus, the marine business of Gurit, also supported Gulf Craft on the engineering for the project. 

Successful sea trials of the Majesty 135 have now been conducted and the yacht is scheduled to be delivered to its owner in April 2012.

Gulf Craft is a global manufacturer of fibreglass luxury yachts with an annual production capacity of around 500 boats. It employs the latest technologies, including sandwich construction and vacuum infusion processes. SP-High Modulus has been working with Gulf Craft for almost 10 and has supplied materials and engineering to other boats in the Majesty range including the 121 and the 125.