The price increase of €100/tonne is effective immediately or at the earliest possible time depending on customer contracts.

Ashland says the pricing action is primarily driven by the continued escalation in costs for key raw materials.

Ashland Performance Materials produces unsaturated polyester resins and epoxy vinyl ester resin, as well as gel-coats and adhesives.