Elantas Europe, a supplier of epoxy resins and adhesives for the manufacturing of composite parts, has been awarded GL (German Lloyd) certification on three of its products, according to its UK supplier Cristex.

EC152 Epoxy Resin with W152.1HR Hardener and W152XLR Hardener, are now GL certified for boat laminating, or composite part laminating.

EC157.1 Epoxy Resin with W152.1HR Hardener and W152XLR Hardener, are GL certified for boat, windmill blade or composite part infusion.

AS90 Epoxy Structural Adhesive with AW91 Hardener and AW93 Hardener, are GL certificated for boat, windmill blade or composite part bonding.

Elantas Europe, a supplier of epoxy resins and adhesives for the manufacturing of composite parts, has been awarded GL (German Lloyd) certification on three of its products, according to its UK supplier Cristex.

  • EC152 Epoxy Resin with W152.1HR Hardener and W152XLR Hardener, are now GL certified for boat laminating, or composite part laminating.
  • EC157.1 Epoxy Resin with W152.1HR Hardener and W152XLR Hardener, are GL certified for boat, windmill blade or composite part infusion.
  • AS90 Epoxy Structural Adhesive with AW91 Hardener and AW93 Hardener, are GL certificated for boat, windmill blade or composite part bonding.

This story is reprinted from material from Cristex, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.