The new Chem-Trend EZ variant provides the same performance as the traditional One FS product for the composites industry, but offers a number of improvements.

Chemlease One FS EZ is a semi-permanent release agent designed for use in the tub / shower, marine, transportation and general composite applications where high gloss finishes are required. Its primary advantage is its ability to be applied quickly, with minimal additional mould surface preparation required to deliver a streak-free or smear-free finished surface. This, along with its durability, results in significantly less time spent in mould preparation while producing a high quality product devoid of imperfections. Once applied, operators merely allow the coating to dry and cure before beginning production.

Additionally, the HAPs free formulation and low odour level contribute to a more environmentally friendly working environment. [HAPS (Hazardous Air Pollutants) are defined under the United States Clean Air Act of 1990 and are designated by the US Environmental Protection Agency.]

Chem-Trend, headquartered in Howell, Michigan, USA, manufactures release agents for use in the composites, rubber, tyre, polyurethane, thermoplastics and die casting industries. It has manufacturing operations in North and South America, Europe and Asia.