Ensinger says that it has commissioned a new facility for the production of thermoplastic prepregs in Cham, Bavaria.

The company now plans to manufacture thermoplastic semipreg materials and fabric-based prepregs at the plant.

Ensinger’s range now includes thermoplastic, continuous fiber-reinforced semipregs and prepregs, organosheets and compression molded composite plates from a range of material.

This story uses material from Ensinger, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.