The Relay manufacturing system enables economical production of lightweight advanced composite structures in high volumes. The station can produce parts with high fibre alignment, high fibre fraction, and long fibre length at high speed with low scrap.

Oribi Manufacturing of Denver, Colorado, USA, will use Fiberforge’s Relay Station to produce advanced composite parts for the outdoor, sporting goods, medical and industrial markets.

Fiberforge is headquartered in Glenwood Springs, Colorado.