FORMAX has been awarded DNV classification for its range of glass multiaxial fabrics.
FORMAX has been awarded DNV classification for its range of glass multiaxial fabrics.

With their complete portfolio of carbon multiaxials having already achieved the same status, the company says that a significant proportion of FORMAX products have now been accredited by the certification body.

FORMAX supplies bespoke, engineered fabrics with different ply weights and orientations to create materials optimised for a diverse range of applications. The Glass Multiaxial range includes a selection of Unidirectional, +/-45 Biaxial, 0/90 Biaxial, Triaxial, and Quadaxial fabrics from weights as low as 250gsm, up to 6000gsm in a variety of fabric widths from 25mm to 2540 mm.