The AVK – Industrievereinigung Verstärkte Kunststoffe eV (Federation of Reinforced Plastics) report illustrates the benefits of FRPs during the entire product lifecycle by analysing four practical examples with regard to their ecological and economical characteristics as well as the social context.

AVK has entered into a partnership with Zajons Zerkleinerungs GmbH. As a licensee, AVK acquired the right to use the label for the CompoCycle recycling system. This offers a method of utilising production waste for AVK members, companies active in the composites market, as well as the public.

This report is available on the AVK website.