GrafTech, headquartered in Parma, Ohio, USA, is a leading provider of graphite and carbon based products and technical and research and development services.

FMI will become part of GrafTech’s Engineered Solutions business.

“FMI adds significant technology in advanced carbon composites to our product portfolio and will aid in propelling continued growth in our Engineered Solutions segment,” comments Craig Shular, Chairman and Chief Executive Officer of GrafTech.

Headquartered in Biddeford, Maine, FMI produces high temperature materials, advanced composites, carbon and graphite insulation and carbon/carbon composite products.