Michelman is known for its Hydrosize® film forming dispersions that can improve the surface chemistry of reinforcement fibers.

The IACMI’s focus is on lowering the cost of advanced fiber-reinforced polymer composite materials by 50%, reducing the energy used to make composites by 75% and increasing the recyclability of composites to more than 95% within the next decade.