Interglas Technologies GmbH is a German producer of technical fabrics for aeronautic, industrial, electrical and building applications.
Interglas Technologies GmbH is a German producer of technical fabrics for aeronautic, industrial, electrical and building applications.

Textiles specialist Porcher Industries has acquired the entire operations of P-D Interglas Technologies.

Interglas Technologies GmbH is a German producer of technical fabrics for aeronautic, industrial, electrical and building applications. Porcher Industries said that this would reinforce its position as a leading global manufacturer of technical textiles, particularly glass fibre fabrics.

Interglas Technologies GmbH, has over 50 years’ experience in the manufacturing and innovation of glass, carbon, basalt, aramid and other synthetic fabrics.

The switchover from P-D Interglas Technologies GmbH to Porcher Industries Germany, started from the beginning of October, with the current Interglas workforce of 155 moving across from this point too.

This story is reprinted from material from Porcherwith editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.