Polynt Composites has raised the price of its UPR and gelcoats by €100/ton.

The company says that it has also raised the price of its range of vinylester by €180/ton.

The price raises will be effective from 15 January or as agreements allow in Europe, the Middle East, and Africa.

According to Polynt, this is due to a ‘further extraordinary escalation of UPRs raw material and logistic cost’. ‘Polynt Composites will continue to work hard to limit the impact of rising costs and raw material availablw upon product pricing and supply,’ a press release said.

This story uses material from Polynt, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.