PPX5 acrylic-based adhesive.
PPX5 acrylic-based adhesive.

SCIGRIP says that this gives assembly engineers an alternative bonding technology for joining low surface energy thermoplastics such as polypropylene or polyethylene.

PPX5 can be used to bond dissimilar plastic substrates (polypropylene, polyethylene, polycarbonate, and PMMA); metals (carbon steel, stainless steel and aluminum); or fibre-reinforced plastics with a minimum of surface preparation to reduce labour costs and production cycle times.

“The PPX5 adhesive was specifically developed for high-performance bonding of these popular thermoplastic polyolefins,” explained Karen Brock Amoah, North American Sales & Marketing Director. “PPX-5 delivers superior bonding properties without the use of solvents or volatile compounds, while requiring minimal surface preparation. In addition, it produces a bond with excellent resistance to water and humid environments, and cures at room temperature.”

While polypropylene and polyethylene plastics are used extensively because of their low cost and durability, they are difficult to bond because their surface properties repel most adhesives. The introduction of the PPX5 acrylic adhesive provides an alternative bonding technology to mechanical assembly or solvent welding.

PPX5 structural adhesive is a two-part acrylic-based plastic bonder designed for application at a 10:1 adhesive/activator mix ratio by volume, with working time of between 2 to 4 minutes, and fixture time of about 90 minutes. The off-white mixed adhesive is resistant to most automotive and industrial solvents, including ethylene glycol, brake fluid, power steering fluid and iso-pentane.

Adhesion properties of the PPX5 adhesive includes a shear strength of 500-870 psi (for thermoplastics); and 500-940 psi (for polyethylene to metals), measured at 75°F/24°C.

The PPX5 adhesive is available in convenient dual-component 50ml cartridges.