Project 12, a composite finishing company based in the UK, says that it has collaborated with Total Composite Solutions on automotive OEM projects for bespoke carbon parts.

TCS is the UK partner of Microtex SRL which makes the clear cosmetic prepreg prepreg used in the projecta, along with Project 12’s coating and carbon fiber substrate surface structure.

‘X4-160 is gaining popularity within the industry due to its clarity, dicy free resin and high TG, enabling flexibility of design application both internally and externally within the vehicle,’ said Michael Stevenson, commercial director of TCS.

This story is reprinted from material from TCS, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.