Cookies enable us to provide the best experience possible and help us understand how visitors use our website. By browsing Materials Today, you agree to our use of cookies.
Knight & Carver Wind Group, a wind turbine blade repair, service and fabrication firm, has entered into a long-term blade service agreement for the North A
The world's longest wind turbine blade – 61.5 m – traveled to be displayed at COP15 in Copenhagen in December last weekend. LM Glasfiber has released a vid
PPG Industries will receive a US$741 000 grant from the US Department of Energy to support the development of materials and automation processes for wind t
Energy Composites Corporation (ECC) has reached agreement with the City of Wisconsin Rapids, Wisconsin, USA, to develop two areas of land into a wind turbi