Cookies enable us to provide the best experience possible and help us understand how visitors use our website. By browsing Materials Today, you agree to our use of cookies.
Suzlon Blade Technology and Idé-Pro Engineering & Software A/S have signed a three year contract under which Idé-Pro will deliver a complete integrated sol
WebCore Technologies LLC has announced that its TYCOR® W core material products have earned a Certificate of Approval by Germanischer Lloyd (GL) for use in
Spirit AeroSystems Inc has shipped the first production leading edge spar component – an outer spar made from carbon composite – for the Airbus A350 XWB pr
Samsung and partners is setting up a wind turbine blade manufacturing plant in Tillsonburg and wind turbine wind tower plant in Windsor, Ontario.
VISTAGY Inc has announced the sale of its FiberSIM® software to Quickstep Technologies Pty Ltd for use in manufacturing composite parts for the newest gene