To meet growing demand for its products, Spirit AeroSystems Inc is to move production of the Boeing 787 Dreamliner fixed leading edge composite wing compon
3B-the fibreglass company is introducing a range of reinforcements designed for specific resin systems used in the manufacture of wind turbine blades. The