Composite materials supplier Cristex Composite Materials has introduced a range of glass fiber fabrics from Italian partners G. Angeloni srl.

Alutex is a range of woven glass fiber fabrics of varied weave patterns. These fabrics are subsequently powder coated using an aluminium powder to create the finished look. As a variation the company can also offer Titanex (dark aluminium), Cuptex (copper) or Goldtex (brass). The new 36 Alutex designs have a weight of 285g/m² up to 365 g/m² and are heavier than the Alutex Fabrics currently available.