Hexcel was recognized for its technology that has contributed significantly to the development of the A350 XWB program for Airbus.
Hexcel was recognized for its technology that has contributed significantly to the development of the A350 XWB program for Airbus.

The award was presented during a dinner held at Queens' College Cambridge, UK on 17 March. 

Hexcel was recognized for its technology that has contributed significantly to the development of the A350 XWB program for Airbus, and for its technology leadership in the region.