MVP's training in Australia.
MVP's training in Australia.

12 distributors from 6 countries attended the three-day training event hosted by Australian distributor MVP-Australia.

The training was exactly the same as the training offered to MVP's customers around the world. It includes classroom instruction on the infusion process and the ins and outs of converting from open moulding to closed moulding using the Flex Molding Process. Hands on training in producing a flexible membrane counter mould and the new Patriot™ Systems developed for Flex Molding are also covered.

All MVP distributors have now completed this course and are ready to assist customers in making the change to the Flex Molding Process.