This service can be used to enhance a customer’s manufacturing capabilities, or to augment their existing capacity for high-volume production.

Norplex-Micarta reports it has already provided contract manufacturing services for numerous material manufacturers.

Norplex-Micarta is equipped with computer controlled treaters, two vertical and six horizontal, and has the capacity to process materials up to 48″ wide. The company has the ability to resin impregnate substrates such as glass, paper, cotton and carbon fibre with epoxy, melamine, phenolic or silicone resins.