Andercol and Scott Bader have expanded their Novascott joint venture plant.
Andercol and Scott Bader have expanded their Novascott joint venture plant.

Composite coating specialists Andercol and Scott Bader say that they have expanded their Novascott joint venture plant, which was established three years ago to meet the needs of the market for gelcoats and composites as well as acrylic resins, low shrinkage resins and structural adhesives.  

The expansion will bring new equipment and new technologies that are not manufactured in Brazil today, the companies says.

‘Brazil presents new perspectives of growth and with the results achieved in different markets such as wind, swimming pools and electricity,’ Scott Bader and Andercol said in a press release. 

This story is reprinted from material from Scott Baderwith editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.