Scott Bader has launched a new range of 3D printing resins for individual consumers and businesses.
Scott Bader has launched a new range of 3D printing resins for individual consumers and businesses.

Scott Bader has launched Crestaform, a new range of 3D printing resins for individual consumers and businesses.

The company says that this is its first ever product range for 3D printing.

Crestaform 3D printing resins can be used in most stereolithography 3D printers and are cured by laser or light.

According to Scott Bader, the resins can achieve a high quality of detail, an improved mechanical performance and improved reactivity.

‘Entering the 3D printing market is an exciting new venture for Scott Bader,’ said Jonathan Stowell, Scott Bader’s commercial director. ‘We have used our in depth experience in resin development to create market leading 3D printing resins that are easy to use and effortlessly produce highly detailed prints.’

This story uses material from Scott Bader, with editorial changes made by Materials Today.