SIGRAPREG TowPreg made from carbon fibers for challenging winding and lay-up processes.
SIGRAPREG TowPreg made from carbon fibers for challenging winding and lay-up processes.

The SIGRAPREG TowPregs have good mechanical properties and permit much more uniform lay-up, the company says. TowPregs can also improve health and safety and environmental protection.

SGL Group has also developed continuous carbon fiber tow for fiber-reinforced thermoplastics and SIGRAPREG prepreg with a newly developed transparent resin system, suitable for visible components in the automotive and other sectors. The use of this prepreg in combination with the SIGRATEX design fabric produces components with improved high surface quality and appearance.