Bindatex has reportedly doubled its capacity by investing in a new slitting line.
Bindatex has reportedly doubled its capacity by investing in a new slitting line.

Composites and materials precision slitting company, Bindatex, has reportedly doubled its capacity by investing in a new slitting line.

The new line has increased Bindatex’s capacity to 30 tonnes per year and has generated five new jobs, Bindatex says. The new line can cut UD, prepreg and composite materials to widths of just 3.175 mm. 

‘This new slitting line has doubled our capacity and allowed us to recruit more staff. It is an exciting time for Bindatex as we expand our company,’ said Bindatex’s MD Chris Lever.